Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 86.2 GPa @Temperature -67.0 °C |
12500 ksi @Temperature -88.6 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP370-8H Fiber Information provided by HexCel |