Polymer Property : Tensile Modulus = 85.5 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 85.5 GPa

@Temperature 77.0 °C
12400 ksi

@Temperature 171 °F
0°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, SGP370-8H Fiber
Information provided by HexCel