Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.40 GPa @Temperature 23.0 °C |
928 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66
(Unverified Data**) Zytel® BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 6.40 GPa @Temperature 60.0 °C |
928 ksi @Temperature 140 °F |
|
LATI Latiblend 6252 H2 G/30 PA6/PP Homopolymer Blend based on Polyamide 6 (PA6) / Polypropylene homopolymer (PPh). Heat stabilized. Glass fibers. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |