Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 36.0 GPa @Temperature 23.0 °C |
5220 ksi @Temperature 73.4 °F |
|
LATI Laramid K/40 HM PPA, 40% Carbon Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Carbon fiber. High tensile modulus. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; .. |