Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 24.1 GPa @Temperature -53.9 °C |
3500 ksi @Temperature -65.0 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Tensile Modulus | 24.1 GPa @Temperature 121 °C |
3500 ksi @Temperature 250 °F |
0° Direction, Wet; ASTM D638 Type 1 |
Park Electrochemical Nelcote® P-670I Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-670I is a versatile, non-styrenated/low VOC polyester resin. P670I is used in a wide variety of applications including radomes, tooling and aircraft structures.Key Features and Benefits:.. |