Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 14.0 GPa @Temperature 23.0 °C |
2030 ksi @Temperature 73.4 °F |
ISO 527 |
Premix Premi-Glas® 1286 Glass Reinforced SMC Description: Premi-Glas® 1286 is a glass reinforced thermoset sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression molding.. |
|||
Tensile Modulus | 14.0 GPa @Temperature 60.0 °C |
2030 ksi @Temperature 140 °F |
|
LATI Laramid G/45 PPA, 45% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Tensile Modulus | 14.0 GPa @Temperature 90.0 °C |
2030 ksi @Temperature 194 °F |
|
LATI Larton G/40 I6 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Good elongation. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Tensile Modulus | 14.0 GPa @Temperature 23.0 °C |
2030 ksi @Temperature 73.4 °F |
|
LATI Latamid SP1 G/50 PA 6.10, 50% Glass Fiber Reinforced Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Tensile Modulus | 14.0 GPa @Temperature 90.0 °C |
2030 ksi @Temperature 194 °F |
|
LATI Latigloss 57 G/50 F2 PPA, 50% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: .. |
|||
Tensile Modulus | 14.0 GPa @Temperature 120 °C |
2030 ksi @Temperature 248 °F |
|
LATI Latilon 28D K/40 PC, 40% Carbon Fiber Reinforced Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b.. |
|||
Tensile Modulus | 14.0 GPa @Temperature 60.0 °C |
2030 ksi @Temperature 140 °F |
|
LATI Latamid 66 H2 K/20 PA 66, 20% Carbon Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Tensile Modulus | 14.0 GPa @Temperature 23.0 °C |
2030 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 70G43HSLA BK099 Nylon 66
(Unverified Data**) Zytel® 70G43HSLA BK099 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 14.0 GPa @Temperature 250 °C |
2030 ksi @Temperature 482 °F |
ISO 527-1 |
Vyncolit Neopreg Kinel® SK4525 S5 Glass Fiber Reinforced Molding Compound BMI molding compound long glass fiber reinforced with excellent mechanical and thermal properties. Especially suited to be used for injection molding.Information provided by Sumitomo Bak North Ameri.. |