Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.9 GPa @Temperature 60.0 °C |
2020 ksi @Temperature 140 °F |
|
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 13.9 GPa @Temperature -40.0 °C |
2020 ksi @Temperature -40.0 °F |
ASTM D638 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |