Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.850 GPa @Temperature 120 °C |
123 ksi @Temperature 248 °F |
|
LATI Latamid 68 H2-V0 PA6/PA66 copolymer, Heat Stabilized, Flame Retardant PA6/PA66 copolymer (PA6/PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Good surface appearance.Availability: Africa & Middle Ea.. |
|||
Tensile Modulus | 0.850 GPa @Temperature 90.0 °C |
123 ksi @Temperature 194 °F |
|
LATI Latan 13 POM Polyoxymethylene (POM). Unfilled. Medium viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Tensile Modulus | 0.850 GPa @Temperature 60.0 °C |
123 ksi @Temperature 140 °F |
|
LATI Latene® 7H2-V2HF PP Homopolymer, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. UL94 V-2 classified, halogens-based flame retardants free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |