Mechanical Properties Metric English Comments
Tensile Modulus 0.800 GPa

@Temperature 90.0 °C
116 ksi

@Temperature 194 °F
LATI Latamid 6 H-V0 PA 6, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good surface appearance.Availability: Africa & Middle East; Asi..
Tensile Modulus 0.800 GPa

@Temperature 120 °C
116 ksi

@Temperature 248 °F
LATI Latamid 66 B H-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. High fluidity. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Blended with PA6.Availability: Africa & Middle East..
Tensile Modulus 0.800 GPa

@Temperature 90.0 °C
116 ksi

@Temperature 194 °F
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin ..
Tensile Modulus 0.800 GPa

@Temperature 60.0 °C
116 ksi

@Temperature 140 °F
LATI Latene® 7H2W-V0 PP Homopolymer, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Low smoke density and low toxicity i..
Tensile Modulus 0.800 GPa

@Temperature 120 °C
116 ksi

@Temperature 248 °F
LATI Latamid 66 S/30 PA 66, 30% Glass Bead Reinforced
Polyamide 66 (PA66) based compound. Glass beads. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Tensile Modulus 0.800 GPa

@Temperature 90.0 °C
116 ksi

@Temperature 194 °F
LATI Latan 23UVE71 POM
Polyoxymethylene (POM). UV stabilized. Toughened. Low viscosity. Good elongation and impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati..
Tensile Modulus 0.800 GPa

@Temperature 90.0 °C
116 ksi

@Temperature 194 °F
LATI Later 4-V0HF1 PBT, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Tensile Modulus 0.800 GPa

@Temperature 23.0 °C
116 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610  (Unverified Data**)
Zytel® RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is a black, unreinforced, toughened and heat stabilised r..
Tensile Modulus 0.800 GPa

@Temperature 23.0 °C
116 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610  (Unverified Data**)
Zytel® RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is an unreinforced and toughened resin for injection molding..
Tensile Modulus 0.800 GPa

@Temperature 260 °C
116 ksi

@Temperature 500 °F
ASTM D 638
Saint-Gobain Meldin® 2001 Bearing
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca..
Copyright © lookpolymers.com All Rights Reserved