Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.550 GPa @Temperature 23.0 °C |
79.8 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h.. |
|||
Tensile Modulus | 0.550 GPa @Temperature 120 °C |
79.8 ksi @Temperature 248 °F |
|
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin .. |
|||
Tensile Modulus | 0.550 GPa @Temperature 60.0 °C |
79.8 ksi @Temperature 140 °F |
|
LATI Latamid 6 BH PA 6, Heat Stabilized Polyamide 6 (PA6). High fluidity. Heat stabilized. Very high fluidity.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Tensile Modulus | 0.550 GPa @Temperature 90.0 °C |
79.8 ksi @Temperature 194 °F |
|
LATI Latene® 7 TR-V2 PP Homopolymer, Mineral Reinforced, Flame Retardant Polypropylene homopolymer (PPh) based compound. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Good surface appearance.Availability: Africa & Middle East; Asia.. |
|||
Tensile Modulus | 0.550 GPa @Temperature 90.0 °C |
79.8 ksi @Temperature 194 °F |
|
LATI Latene® 7H2-V2HF PP Homopolymer, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. UL94 V-2 classified, halogens-based flame retardants free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Tensile Modulus | 0.550 GPa @Temperature 60.0 °C |
79.8 ksi @Temperature 140 °F |
|
LATI Latene® EP 7-V2HF PP Copolymer, Flame Retardant Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; N.. |