Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 601.2 MPa @Thickness 4.80 - 25.4 mm, Temperature 538 °C |
87200 psi @Thickness 0.189 - 1.00 in, Temperature 1000 °F |
|
Haynes Hastelloy® C-276 alloy, solution heat treated flat products Hastelloy® C-276 alloy is a nickel-molybdenum-chromium wrought alloy that is a versatile corrosion-resistant alloy. C-276 alloy is an improved wrought version of alloy C in that it usually doesn'.. |