Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 570 MPa @Temperature 371 °C |
82700 psi @Temperature 700 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Tensile Strength, Ultimate | 570 MPa @Temperature 650 °C |
82700 psi @Temperature 1200 °F |
Solution Annealed prior to test |
Special Metals INCONEL® Alloy 617 A nickel-chromium-cobalt-molybdenum alloy with an exceptional combination of metallurgical stability, strength, and oxidation resistance at high temperatures. Resistance to oxidation is enhanced by.. |
|||
Tensile Strength, Ultimate | 570 MPa @Temperature 371 °C |
82700 psi @Temperature 700 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |