Polymer Property : Tensile Strength, Ultimate = 3000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.7 MPa

@Thickness 1.00 - 6.00 mm
3000 psi

@Thickness 0.0394 - 0.236 in
ASTM D638
CPC - Vycom CELTEC® Expanded Rigid foam PVC board
Celtec Displayboard is a foamed polyvinyl chloride (PVC) sheet whose combination of features makes it ideal for signage, exhibits, store displays, POP, Kiosks, screen printing and more. The surface..