Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 194 MPa @Temperature 260 °C |
28100 psi @Temperature 500 °F |
short term exposure |
CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition AMC225xe is a high quality aerospace grade aluminum alloy (AA2124) reinforced with 25% by volume of ultrafine particles of silicon carbide. It is manufactured by a special powder metallurgy route us.. |