Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1200 MPa @Temperature 23.0 °C |
174000 psi @Temperature 73.4 °F |
|
Special Metals NIMONIC® Alloy 901 A nickel-iron-chromium alloy containing titanium and aluminum for precipitation hardening and molybdenum for solid-solution strengthening. The alloy has high yield strength and creep resistance at .. |
|||
Tensile Strength, Ultimate | 1200 - 1590 MPa @Temperature 20.0 °C |
174000 - 231000 psi @Temperature 68.0 °F |
varies with heat treatment |
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
Tensile Strength, Ultimate | 1200 - 1590 MPa @Temperature 20.0 °C |
174000 - 231000 psi @Temperature 68.0 °F |
varies with heat treatment |
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava.. |
|||
Tensile Strength, Ultimate | 1200 - 1590 MPa @Temperature 20.0 °C |
174000 - 231000 psi @Temperature 68.0 °F |
varies with heat treatment |
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits wat.. |