Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1100 MPa @Temperature 400 °C |
160000 psi @Temperature 752 °F |
|
International Mold Steel DH2F Pre-Hardened H13-Type Mold Steel Description: DH2F is one of the best machining pre-hardened H13-type steels available.Unique Characteristics: 38-42 HRc hardness.Through hardened for exceptional dimensional stability.Cuts mold maki.. |
|||
Tensile Strength, Ultimate | 1103 MPa @Temperature 300 °C |
160000 psi @Temperature 572 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Tensile Strength, Ultimate | 1100 MPa @Temperature 650 °C |
160000 psi @Temperature 1200 °F |
Precipitation Hardened prior to test |
Special Metals INCONEL® Alloy 718 Developed in the early 1960's, IN718 is still considered the material of choice for the majority of aircraft engine components with service temperatures below 1200°F (650°C). Inconel 718 is a.. |
|||
Tensile Strength, Ultimate | 1100 MPa @Temperature 23.0 °C |
160000 psi @Temperature 73.4 °F |
|
Special Metals MONEL® Alloy K-500 A precipitation-hardenable nickel-copper alloy that combines the corrosion resistance of MONEL alloy 400 with greater strength and hardness. It also has low permeability and is nonmagnetic to under.. |
|||
Tensile Strength, Ultimate | 1100 - 1380 MPa @Temperature 315 °C |
160000 - 200000 psi @Temperature 599 °F |
varies with heat treatment |
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
Tensile Strength, Ultimate | 1100 - 1380 MPa @Temperature 315 °C |
160000 - 200000 psi @Temperature 599 °F |
varies with heat treatment |
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava.. |
|||
Tensile Strength, Ultimate | 1100 - 1380 MPa @Temperature 315 °C |
160000 - 200000 psi @Temperature 599 °F |
varies with heat treatment |
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits wat.. |