Polymer Property : Tensile Strength, Ultimate = 950 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 800 - 950 MPa

@Diameter 101 - 210 mm
116000 - 138000 psi

@Diameter 3.98 - 8.27 in
Rm., un-machined
Assab Steels 709M Machinery Steel
ASSAB 709M is an alloyed machinery steel with high strength in small and medium sizes. As standard ASSAB 705M is supplied tough hardened requiring no further heat treatment. It can be oil hardened t..