Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 864 MPa @Thickness 12.7 mm, Temperature 20.0 °C |
125000 psi @Thickness 0.500 in, Temperature 68.0 °F |
|
Haynes Hastelloy® S alloy, flat products Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |