Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 792.2 MPa @Thickness 2.00 mm, Temperature 20.0 °C |
114900 psi @Thickness 0.0787 in, Temperature 68.0 °F |
|
Haynes Hastelloy® C-276 alloy, solution heat treated flat products Hastelloy® C-276 alloy is a nickel-molybdenum-chromium wrought alloy that is a versatile corrosion-resistant alloy. C-276 alloy is an improved wrought version of alloy C in that it usually doesn'.. |