Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 767 MPa @Temperature 100 °C |
111000 psi @Temperature 212 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Tensile Strength, Ultimate | 767 MPa @Thickness 6.30 mm, Temperature 20.0 °C |
111000 psi @Thickness 0.248 in, Temperature 68.0 °F |
|
Haynes Hastelloy® C-4 alloy, plate, heat treated at 1066°C, rapid quenched Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |