Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 643 MPa @Thickness 9.50 mm, Temperature 538 °C |
93300 psi @Thickness 0.374 in, Temperature 1000 °F |
|
Haynes Hastelloy® C-4 alloy, plate, heat treated at 1066°C, rapid quenched Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
Tensile Strength, Ultimate | 643 MPa @Thickness 3.20 mm, Temperature 538 °C |
93300 psi @Thickness 0.126 in, Temperature 1000 °F |
|
Haynes Hastelloy® C-4 alloy, sheet, aged 100 hours at 899°C Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |