Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 517 MPa @Temperature 816 °C |
75000 psi @Temperature 1500 °F |
|
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy pr.. |
|||
Tensile Strength, Ultimate | 517 MPa @Temperature 816 °C |
75000 psi @Temperature 1500 °F |
|
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy pr.. |