Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 262 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 262 MPa

@Temperature 316 °C
38000 psi

@Temperature 600 °F
18-8 stainless steel butt joint.
Lucas-Milhaupt BRAZE 403 Carbide Brazing Alloy
Applications: Braze 403 is a good intermediate temperature brazing alloy for use on stainless steels, mild steels, cast and malleable irons and various nonferrous alloys. This alloy is particularly..
Tensile Strength, Ultimate 262 MPa

@Temperature 260 °C
38000 psi

@Temperature 500 °F
Inconel butt joint
Lucas-Milhaupt EASY FLO 45 Silver Based Cadmium-Bearing Filler Metal
Applications: Easy-Flo 45 is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wet..