Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.877 - 1.05 kN/m | 5.00 - 6.00 pli | Adhesion to Aluminum, etched |
3M Controltac™ 180Cv2-10 Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |
|||
Peel Strength | 0.526 - 1.05 kN/m | 3.00 - 6.00 pli | Adhesion to Powder coat paint |
3M Controltac™ 3690C Graphic Film with Comply™ Adhesive This is a 2-mil white, clear or black film for screen printing graphics. The aggressive, pressure activated-adhesive is slideable and repositionable, and has air release channels for fast and easy b.. |
|||
Peel Strength | 0.877 - 1.05 kN/m | 5.00 - 6.00 pli | Adhesion to Aluminum, etched |
3M Controltac™ FN180C-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 0.526 - 1.05 kN/m | 3.00 - 6.00 pli | Adhesion to Powder coat paint |
3M Scotchcal™ 3690 Graphic Film This is a 2-mil white for black film for screen printing graphics. The aggressive, pressure sensitive-adhesive is well suited for graphics applied to sand cast, moderately rough surfaces and some lo.. |
|||
Peel Strength | 0.526 - 1.05 kN/m | 3.00 - 6.00 pli | Adhesion to Powder coat paint |
3M Scotchcal™ 3690LF Graphic Film This is a 2-mil white for black film for screen printing graphics. The aggressive, pressure sensitive-adhesive is well suited for graphics applied to sand cast, moderately rough surfaces and some lo.. |
|||
Peel Strength | 0.701 - 1.05 kN/m | 4.00 - 6.00 pli | Adhesion to Fruehauf pre-painted panel |
3M Scotchcal™ IJ780Cv3 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-sensitive adhesive with non-visible, air release channels for fast, easy, bubble-free installations; Confirms to flat s.. |
|||
Peel Strength | 0.877 - 1.05 kN/m | 5.00 - 6.00 pli | Adhesion to Acrylic |
3M Scotchcal™ IJ780Cv3 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-sensitive adhesive with non-visible, air release channels for fast, easy, bubble-free installations; Confirms to flat s.. |
|||
Peel Strength | 0.877 - 1.05 kN/m | 5.00 - 6.00 pli | Adhesion to Aluminum, etched |
3M Controltac™ 180C Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |
|||
Peel Strength | 0.877 - 1.05 kN/m | 5.00 - 6.00 pli | Adhesion to Aluminum, etched |
3M Controltac™ FN180Cv3-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 0.877 - 1.05 kN/m | 5.00 - 6.00 pli | Adhesion to Aluminum, etched |
3M Controltac™ IJ180-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 0.877 - 1.05 kN/m | 5.00 - 6.00 pli | Adhesion to Aluminum, etched |
3M Controltac™ IJ180C-10 Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 0.877 - 1.05 kN/m | 5.00 - 6.00 pli | Adhesion to Aluminum, etched |
3M Controltac™ IJ180Cv3-10 Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 0.877 - 1.05 kN/m | 5.00 - 6.00 pli | Adhesion to Aluminum, etched |
3M Controltac™ RG180-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 0.877 - 1.05 kN/m | 5.00 - 6.00 pli | Adhesion to Aluminum, etched |
3M Controltac™ RG180C-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 0.701 - 1.05 kN/m | 4.00 - 6.00 pli | Adhesion to Aluminum, etched |
3M Envision™ 480Cv3 Print Wrap Film High performance, 2-mil white, non-PVC film with a luster finish; Pressure-act adhesive for easy sliding, tacking, snap up and repositioning; non-visible air release channels for fast and easy, bubb.. |
|||
Peel Strength | 0.877 - 1.05 kN/m | 5.00 - 6.00 pli | Adhesion to Aluminum, etched |
3M Controltac™ 180 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |