Mechanical Properties Metric English Comments
Peel Strength 1.2819 kN/m
7.3125 pli
to Stainless Steel, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330
3M 9589 Double Coated Tapes with Adhesive 700 Series
3M™ Double Coated Tapes with 3M™ Adhesive 700 Series feature a high tack synthetic rubber adhesive which provides excellent quick stick or initial adhesion and bonds together a wide variety of mat..