Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.23 kN/m | 7.00 pli | Al/Al, 30 min cure at 175°F |
Master Bond Supreme 3HT-80 One Component, Toughened, Heat Curing Epoxy Master Bond Polymer System Supreme 3HT-80 is a one component, heat curing epoxy adhesive/sealant featuring excellent physical and chemical resistance properties and a minimal curing temperature of 1.. |
|||
Peel Strength | 1.23 kN/m | 7.00 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon 51588R015 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1 Layer 2: Uncured Silicone RubberSide 1 Layer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPETh.. |
|||
Peel Strength | 1.23 kN/m | 7.00 pli | To Copper (1 oz./35 micron); After Process Solutions; IPC TM-650 2.4.8 |
Arlon CLTE Microwave Printed Circuit Board Substrate CLTE is a ceramic powder-filled and woven micro fiberglass reinforced PTFE composite engineered to produce a stable, low water absorption laminate with a nominal Dielectric Constant of 2.98.Ceramic/.. |
|||
Peel Strength | 1.23 kN/m | 7.00 pli | To Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8 |
Arlon CLTE Microwave Printed Circuit Board Substrate CLTE is a ceramic powder-filled and woven micro fiberglass reinforced PTFE composite engineered to produce a stable, low water absorption laminate with a nominal Dielectric Constant of 2.98.Ceramic/.. |
|||
Peel Strength | 1.23 kN/m | 7.00 pli | After Thermal Stress; IPC TM-650 2.4.8 |
Arlon CLTE-P Pre-Preg Bonding Layer Arlon's CLTE-P Prepreg Bonding Layer is a ceramic filled PTFE coated glass stock that is used as a bonding ply for CLTE, CLTE-X or CLTE-AT laminates. CLTE-P is a pre-preg material that consists of .. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ 180Cv2-10 Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ FN180C-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 1.23 kN/m | 7.00 pli | |
Arlon TC350 Glass, PTFE and Micro-Dispersed Ceramic High Thermal Conductivity, Excellent Dielectric Constant Control and Phase Stability with TemperatureInformation provided by Arlon Materials for Electronics (MED). |
|||
Peel Strength | 1.23 kN/m | 7.00 pli | Adhesion to PE; ASTM D1000 |
3M Scotch® 31 Heavy Duty Mining Tape Scotch® Heavy Duty Mining Tape 31 has a tough, abrasion-resistant backing for jacket repair on mining cables. Due to extremely abrasive environment, the original jacket on the cable gets damaged of.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, etched |
3M Scotchcal™ IJ780Cv3 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-sensitive adhesive with non-visible, air release channels for fast, easy, bubble-free installations; Confirms to flat s.. |
|||
Peel Strength | 1.23 kN/m @Temperature 66.0 °C, Time 1.21e+6 sec |
7.00 pli @Temperature 151 °F, Time 336 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 4491 Vinyl Bonding Cylinder Spray Adhesive Industrial grade, high performance, plasticizer resistant bulk spray adhesive formulated for bonding vinyl. The adhesive is available in a convenient, portable, no maintenance aerosol cylinder.Infor.. |
|||
Peel Strength | 1.23 kN/m @Temperature 82.0 °C |
7.00 pli @Temperature 180 °F |
Bell Pell Adhesion, Aluminum Etched, Adhesive Failure; ASTM D3167 |
3M Scotch-Weld™ DP920 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i.. |
|||
Peel Strength | 1.23 kN/m | 7.00 pli | Backside, to Stainless Steel, 180° Peel, 2 mil Al |
3M XT6110 Hi-Tack Double Coated Tape 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product construction to support demanding application requirements. This product line provides a range of.. |
|||
Peel Strength | 1.23 kN/m | 7.00 pli | Bond Strength; Arlon-SQA-TMS-011 |
Arlon 51271R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneProduct Use: Flexible heater in.. |
|||
Peel Strength | >= 1.23 kN/m | >= 7.00 pli | Bond Strength |
Arlon R31861R018 0.018" (0.457 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ 180C Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ FN180Cv3-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ IJ180-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ IJ180C-10 Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ IJ180Cv3-10 Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ IJ380Cv3 Wrap Film with Comply™ v3 Adhesive 2-mil white, vinyl film with a luster finish; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Non-visible, air release channels for fast, easy, bubble-free installa.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ RG180-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 1.23 kN/m | 7.00 pli | to Stainless Steel; ASTM D3330 |
3M VHB™ F9460PC Adhesive Transfer Tapes with Adhesive 100MP 3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng.. |
|||
Peel Strength | 1.23 kN/m | 7.00 pli | 90° Peel, PET/Stainless Steel, 72 hrs at RT; ASTM D3330 |
3M 9045MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 1.23 kN/m | 7.00 pli | at elevated temperature; IPC-TM-650.2.4.8.2a |
Park Electrochemical Nelco® N4000-11 BC® Buried Capacitance™ Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |
|||
Peel Strength | 1.23 kN/m | 7.00 pli | at elevated temperature; IPC-TM-650.2.4.8.2a |
Park Electrochemical Nelco® N4000-6 FC Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-6 FC is a high-Tg epoxy laminate and prepreg system that provides a wide range of performance versatility and ease of processing for demanding high-layer count applications.Key Fea.. |
|||
Peel Strength | 1.23 kN/m | 7.00 pli | Steel-Unsupported Vinyl, 180°, Aging 1 Day @ RT |
3M Scotch-Weld™ 2262 Plastic Adhesive Features:It is a high strength adhesive with exceptional resistance to plasticizer migration and bonds vinyl extrusions, flexible and rigid vinylsIt dries clear, is non-staining and features a very .. |
|||
Peel Strength | 1.23 kN/m | 7.00 pli | on canvas |
3M Scotch-Weld™ 3762 Hot Melt Adhesive Excellent “hot tack”, fast setting corrugated, beadboard, recouperage, repacking chipboard, wood and Economical, general purposeInformation provided by 3M |
|||
Peel Strength | 1.23 kN/m | 7.00 pli | at elevated temperature; IPC-TM-650.2.4.8.2a |
Park Electrochemical Nelco® N4000-11 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |