Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 9.12 kN/m @Temperature 21.1 °C |
52.0 pli @Temperature 70.0 °F |
Bell Peel |
Hexcel® Redux® 312 Modified epoxy film adhesive (0.06 psf) Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support.. |
|||
Peel Strength | 9.12 kN/m @Temperature 21.1 °C |
52.0 pli @Temperature 70.0 °F |
Bell Peel |
Hexcel® Redux® 312UL Modified epoxy film adhesive Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support.. |
|||
Peel Strength | 9.12 kN/m @Temperature 21.1 °C |
52.0 pli @Temperature 70.0 °F |
|
Hexcel® Redux® 335K Adhesive film for bonding metallic and composite components (0.03 psf) Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a.. |
|||
Peel Strength | 9.12 kN/m @Temperature 21.1 °C |
52.0 pli @Temperature 70.0 °F |
|
Hexcel® Redux® 335U Adhesive film for bonding metallic and composite components (0.03 psf) Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a.. |
|||
Peel Strength | 9.12 kN/m | 52.0 pli | 90°, Adhesion to Polypropylene |
3M Bumpon™ SJ5208 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 9.12 kN/m | 52.0 pli | 90°, Adhesion to Polypropylene |
3M Bumpon™ SJ5216 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 9.12 kN/m | 52.0 pli | 90°, Adhesion to Polypropylene |
3M Bumpon™ SJ6216 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 9.12 kN/m | 52.0 pli | 180°, Aluminum |
3M Scotch-Weld™ TE040 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 9.12 kN/m | 52.0 pli | 90°, Adhesion to Polypropylene |
3M SJ5201 Protective Product, Die Cut Shapes 3M Bumpon Protective Products SJ5201 and SJ5202 are pressure-sensitive, adhesive backed polyurethane products made from SJ5200 Series soft foam rollstock. A hexagon shape is often preferred for vari.. |
|||
Peel Strength | 9.12 kN/m | 52.0 pli | 90°, Adhesion to Polypropylene |
3M SJ6100 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 9.12 kN/m | 52.0 pli | 90°, Adhesion to Polypropylene |
3M SJ6344 Protective Product, Molded Shapes 3M Bumpon Protective Products SJ6344 is a pressure-sensitive adhesive-backed, molded polyurethane product. The Bumpon SJ6344 is called an Easy Slide Series because it incorporates a special abrasion.. |
|||
Peel Strength | 9.12 kN/m | 52.0 pli | 90°, Adhesion to Polypropylene |
3M Bumpon™ SJ6208 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 9.12 kN/m | 52.0 pli | 90°, Adhesion to Polypropylene |
3M Bumpon™ SJ6232 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 9.12 kN/m | 52.0 pli | 90°, Adhesion to Polypropylene |