Mechanical Properties Metric English Comments
Peel Strength 8.77 kN/m
50.0 pli
Tensile
Dielectric Polymers NT-4512 High Temperature Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film. For applicati..
Peel Strength 8.77 kN/m
50.0 pli
Tensile
Dielectric Polymers NT-2821 Ultra Tack Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film at zero wet out..
Peel Strength 8.77 kN/m
50.0 pli
Tensile
Dielectric Polymers NT-2821-2 Ultra Tack Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film at zero wet out..
Peel Strength 8.77 kN/m
50.0 pli
Tensile
Dielectric Polymers NT-2822 Ultra Tack Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film at zero wet out..
Peel Strength 8.77 kN/m
50.0 pli
Tensile
Dielectric Polymers NT-2012-2 Photo Processing Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing photographic film to leader card during film proc..
Peel Strength 8.77 kN/m
50.0 pli
Tensile
Dielectric Polymers NT-5521-2 Photo Processing Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing photographic film to leader card during film proc..
Peel Strength 8.77 kN/m
50.0 pli
Tensile
Dielectric Polymers NT-8512-2 Photo Processing Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing photographic film to leader card during film proc..
Peel Strength 8.77 kN/m
50.0 pli
Tensile
Dielectric Polymers NT-702 Acrylic Tape  (discontinued **)
Acrylic adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of non-silicone coated substrates. Provides high temperature s..
Peel Strength 8.77 kN/m
50.0 pli
Tensile
Dielectric Polymers NT-5000 Protective Film  (discontinued **)
Acrylic adhesive with polyester film backing.Features: Clean removal even after exposure to high and low temperaturesSolvent resistantMoisture resistantFor use on matte metals and textured plasticsA..
Peel Strength 8.77 kN/m
50.0 pli
Tensile
Dielectric Polymers NT-8512-2 Powder Coating Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityNo film shrinkage after exposure to elevated temperaturesAbrasion resista..
Peel Strength 8.77 kN/m
50.0 pli
Tensile
Dielectric Polymers NT-9512 Powder Coating Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityNo film shrinkage after exposure to elevated temperaturesAbrasion resista..
Peel Strength 8.77 kN/m
50.0 pli
Tensile
Dielectric Polymers NT-9512-2DL Selective Masking Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: High temperature resistantDie cut disks/shapes remove easily from linerClean tape removalApplications: For selective masking appli..
Peel Strength 8.77 kN/m
50.0 pli
ITW Devcon Flex Bondâ„¢ Methacrylate Adhesive Pipe Sealant, Purple
Information provided by ITW Devcon
Peel Strength 8.77 kN/m
50.0 pli
ITW Devcon Safety Clear Coatâ„¢ Epoxy, Water Clear
Information provided by ITW Devcon
Peel Strength 8.77 kN/m
50.0 pli
At 100% cohesive failure using 1 in. x 8 in. stainless steel screen at 180° pull angle
Momentive Performance Materials RTV1673LV One Component, Low Volatile Silicone Adhesive Sealant, Black
RTV1673LV one-component, ready-to-use adhesive sealants cures to a tough durable, resilient silicone rubber when exposed to atmospheric moisture at room temperature. Methyl alcohol and a small amoun..
Peel Strength 8.77 kN/m

@Temperature 21.1 °C
50.0 pli

@Temperature 70.0 °F
Hexcel® Redux® 335U Adhesive film for bonding metallic and composite components (0.06 psf)
Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a..
Peel Strength 8.77 kN/m
50.0 pli
Aluminum Etched, T-Peel, 17-20 mil bondline
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Peel Strength 8.77 kN/m

@Temperature 23.0 °C
50.0 pli

@Temperature 73.4 °F
Aluminum, T-Peel
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Peel Strength 8.77 kN/m
50.0 pli
T-Peel, CRS Oakite degreased, 5-8 mil bondline
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Peel Strength 8.77 kN/m
50.0 pli
Solvent Wiped T-Peel
3M Scotch-Weld™ EC-2086 Structural Adhesive
3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M
Peel Strength 8.77 kN/m
50.0 pli
180°, Polystyrene
3M Scotch-Weld™ TS230 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Peel Strength 8.77 kN/m
50.0 pli
180°, Polyacrylic
3M Scotch-Weld™ EZ250150 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th..
Peel Strength 8.77 kN/m
50.0 pli
180°, Aluminum
3M Scotch-Weld™ EZ250150 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th..
Peel Strength 8.77 kN/m
50.0 pli
Aluminum Etched, T-Peel, 5-8 mil bondline
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Peel Strength 8.77 kN/m

@Temperature 23.0 °C
50.0 pli

@Temperature 73.4 °F
Aluminum, T-Peel
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Peel Strength 8.77 kN/m
50.0 pli
Tensile
Dielectric Polymers NT-5002 Protective Film  (discontinued **)
Acrylic adhesive with polyester film backing.Features: Clean removal even after exposure to high and low temperaturesSolvent resistantMoisture resistantFor use on matte metals and textured plasticsA..
Copyright © lookpolymers.com All Rights Reserved