Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.877 kN/m | 5.00 pli | Copper, After Solder Float, 1/2 ounce TCR Foil; IPC-TM-650 2.4.8 |
Rogers Corporation RO4350B Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil RO4000® Series High Frequency Circuit Materials are glass-reinforced hydrocarbon and ceramic (not PTFE) laminates with TICER™ TCR® Thin Film Resistor Foils. These laminates are designed for perf.. |
|||
Peel Strength | 0.877 - 1.75 kN/m | 5.00 - 10.0 pli | T-peel, Al to Al |
Master Bond Supreme 10AOHT-LO High Shear and Peel Strength Epoxy Description: Master Bond Supreme 10AOHT-LO has a combination of properties consisting of excellent thermal conductivity, superior electrical insulation, great adhesion to a wide variety of substrate.. |
|||
Peel Strength | >= 0.877 kN/m | >= 5.00 pli | T-peel, Al to Al |
Master Bond Supreme 10HTFS Silver Conductive Microelectronic Epoxy Description: Master Bond Polymer System Supreme 10HTFS “snap cure” epoxy is a formulated system featuring a combination of high performance properties including high shear and peel strength, outst.. |
|||
Peel Strength | 0.877 - 5.26 kN/m | 5.00 - 30.0 pli | Varies with substrates. |
Loctite® Durabond® E-20NS Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Peel Strength | 0.877 - 5.26 kN/m | 5.00 - 30.0 pli | Varies with substrates. |
Loctite® Durabond® E-30CL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Peel Strength | >= 0.877 kN/m | >= 5.00 pli | Bond Strength |
Arlon 57226R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Linered side-Photopolymer, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1015 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP026009 White Polypropylene Label Product 3M™ White Polypropylene Label Products FP022101, FP022102, FP022108, FP026002, FP02600N and FP026009 are matte white opaque materials that offer excellent durability and moisture resistance. These .. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP032708 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are clear materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1480, which is a high performance tac.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ 1000-17 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Alodine, aluminum |
3M Scotchcal™ 50-24 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Alodine, aluminum |
3M Scotchcal™ 50-73 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7125-10 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7125-114 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7125-90 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7125-96 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7725-193 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | T-Peel, Steel Solvent Wipe; ASTM D1876-61T |
3M Scotch-Weld™ 1751 B/A Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1751 B/A is a gray, aluminum filled, two-part, room temperature curing structural adhesive.Information provided by 3M |
|||
Peel Strength | >= 0.877 kN/m | >= 5.00 pli | Bond Strength |
Arlon 44566R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w.. |
|||
Peel Strength | >= 0.877 kN/m | >= 5.00 pli | [ppi], Bond Strength |
Arlon 47576R009 0.0095" (0.241 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured RubberSide 2: Uncured RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production material. The data sho.. |
|||
Peel Strength | >= 0.877 kN/m | >= 5.00 pli | Bond Strength |
Arlon 51571S020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Glass, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7907 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat.. |
|||
Peel Strength | >= 0.877 kN/m | >= 5.00 pli | Bond vs. Copper Foil (no Primer) |
Arlon R33889R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Layer-on-Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information .. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM041902 White Polyester Label Products 3M™ White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive P1480, which .. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7125-22 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7125-54 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7725-77 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ 1000-53 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |