Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 8.59 kN/m @Temperature 21.1 °C |
49.0 pli @Temperature 70.0 °F |
|
Hexcel® Redux® 335M Adhesive film for bonding metallic and composite components (0.03 psf) Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a.. |