Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.789 kN/m | 4.50 pli | 180° peel, PET/s.s. |
Dielectric Polymers NT-140APS General Purpose Laminating Adhesive
(discontinued **) Acrylic adhesive with moisture stable PE coated kraft (60#) liner.Features: Plasticizer migration resistantChemical resistantMoisture resistantApplications: Mounting nameplates, signs, graphic panel.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | 180° peel, PET/s.s. |
Dielectric Polymers NT-140A89 General Purpose Laminating Adhesive
(discontinued **) Acrylic adhesive with moisture stable PE coated kraft (89#) liner.Features: Plasticizer migration resistantChemical resistantMoisture resistantApplications: Mounting nameplates, signs, graphic panel.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | 180° peel, PET/s.s. |
Dielectric Polymers NT-240APS High Temperature Laminating Adhesive
(discontinued **) Acrylic adhesive with moisture stable PE coated kraft (60#) liner.Features: Plasticizer migration resistantHigh temperature shear propertiesNeutral pHSolvent resistantApplications: Interior automoti.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7600 Removable Vinyl Label Material 3M™ Removable Vinyl Label Material 7600 is a conformable white vinyl stock that utilizes 3M™ Adhesive 500 which offers clean removability on most surfaces for up to one year, as well as, excellent.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | PVC, 180°, after 48 hrs at 23°C |
3M Fastbond™ 49 Insulation Adhesive 3M™ Fastbond™ Insulation Adhesive 49 is a water-based, high solids, fast tacking, pressure sensitive adhesive for bonding lightweight materials like fiberglass insulation, felt, shoddy, paper and .. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP032302 White Metallized Polypropylene Label Products 3M™ White Metallized Polypropylene Label Products FP032302, FP032302W and FP032305 are a white opaque material that offers excellent durability and opacity. These label products utilize 3M™ Adhesi.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP032302W White Metallized Polypropylene Label Products 3M™ White Metallized Polypropylene Label Products FP032302, FP032302W and FP032305 are a white opaque material that offers excellent durability and opacity. These label products utilize 3M™ Adhesi.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 5100 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Permanent; Available in 15 colors, including black (which reflects whit.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 680-10 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 680-14 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 680-72 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 680-75 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ IJ680-10 Reflective Graphic Film 6-mil flexible, enclosed lens, retroreflective films; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity when wet; Excellent angularity; Pressure.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ RG680-10 Reflective Graphic Film 6-mil flexible, enclosed lens, retroreflective films; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity when wet; Excellent angularity; Pressure.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | Polycarbonate, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7053 Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products 7046 and 7053 are durable, high performance materials that offer excellent durability and moisture resistance. These vinyl label stocks utilize.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7908FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | 90° Peel, PET/Polycarbonate, 72 hrs at 70°C; ASTM D3330 |
3M 7957MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | 90° Peel, PET/PET, 72 hrs at 70°C; ASTM D3330 |
3M 7993MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 680-76 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7884 White Vinyl Label Material Features:Conformable to contoured surfacesResists wrinkling and delaminationOne-piece removal up to one year after applicationTopcoated for impact printing, typewriters, ballpoint pens, pencils, and.. |
|||
Peel Strength | 0.789 kN/m | 4.50 pli | 90° Peel, PET/Polycarbonate, 72 hrs at RT; ASTM D3330 |
3M 9045MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |