Polymer Property : Peel Strength = 4.33 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.759 kN/m
4.33 pli
Non-linered side-Composite Sleeve, Adhesion; ASTM D3330
3M Cushion-Mount™ E1920 Plus Plate Mounting Tapes with Easy Mount Adhesive
3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel..