Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.701 kN/m | 4.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP017102 White Polyester Label Products 3M™ White Polypropylene Label Products FP017102 and FP026508 offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a general purpose permane.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP019808 White Polyester Label Products 3M™ White Polypropylene Label Products FP019802 and FP019808 offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is for labeling tires when u.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Urethane paints |
3M Scotchcal™ 1000-41 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Acrylic enamel |
3M Scotchcal™ 1000LF-114 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Fruehauf pre-painted panels |
3M Scotchcal™ 8626 ES Clear Graphic Film Film 8626 ES is a 2 mil, clear graphic film with pressure-sensitive adhesive. It is designed for flat, single or multi-layered internally illuminated signs or window graphics, both indoors and outdo.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to ABS |
3M Scotchcal™ ElectroCut™ 7125-105 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Acrylic enamel |
3M Scotchcal™ ElectroCut™ 7125-177 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Polycarbonate |
3M Scotchcal™ ElectroCut™ 7125-186 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Fruehauf pre-painted panels |
3M Scotchcal™ ElectroCut™ 7125-25 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to ABS |
3M Scotchcal™ ElectroCut™ 7125-57 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Acrylic |
3M Scotchcal™ ElectroCut™ 7125-63 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Acrylic |
3M Scotchcal™ ElectroCut™ 7125-99 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Polycarbonate |
3M Scotchcal™ ElectroCut™ 7725-10 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Fruehauf pre-painted panels |
3M Scotchcal™ ElectroCut™ 7725-176 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Urethane paints |
3M Scotchcal™ ElectroCut™ 7725-193 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to ABS |
3M Scotchcal™ ElectroCut™ 7725-197 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Acrylic |
3M Scotchcal™ ElectroCut™ 7725-63 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Fruehauf pre-painted panels |
3M Scotchcal™ ElectroCut™ 7725-89 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.701 - 0.877 kN/m | 4.00 - 5.00 pli | Adhesion to ABS |
3M Scotchcal™ IJ780Cv3 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-sensitive adhesive with non-visible, air release channels for fast, easy, bubble-free installations; Confirms to flat s.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Stainless Steel, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7025 Screen Printable Polyester Performance Label Products 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer good thermal stability and moisture resistance. These topcoated polyester label stocks u.. |
|||
Peel Strength | 0.701 - 0.877 kN/m | 4.00 - 5.00 pli | Adhesion to ABS |
3M Controltac™ RG180-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Fruehauf pre-painted panels |
3M Scotchcal™ ElectroCut™ 7125-31 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Acrylic |
3M Scotchcal™ ElectroCut™ 7125-39 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to ABS |
3M Scotchcal™ ElectroCut™ 7125-48 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Fruehauf pre-painted panels |
3M Scotchcal™ ElectroCut™ 7725-276 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Urethane paints |
3M Scotchcal™ ElectroCut™ 7725-29 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Polycarbonate |
3M Scotchcal™ ElectroCut™ 7725-38 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Acrylic enamel |
3M Scotchcal™ ElectroCut™ 7725-47 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Acrylic and uncoated, clear polycarbonate |
3M Scotchcal™ 3632-76 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Polycarbonate |
3M Scotchcal™ ElectroCut™ 405 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |