Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 4.38 kN/m | 25.0 pli | At 100% cohesive failure using 1 in. x 8 in. stainless steel screen at 180° pull angle |
Momentive Performance Materials RTV116 One Component Acetoxy Adhesive Sealant, Red RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | T-peel |
Master Bond EP21TDCHTND Versatile, toughened two component epoxy for bonding, sealing and coating Product Description: Master Bond EP21TDCHTND is a two component epoxy adhesive, sealant and coating featuring high performance, versatility and exceptional user friendliness. It has a very forgiving.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | Bond Strength; ASTM D624 |
Arlon 49481R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical .. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Polystyrene |
3M Bumpon™ SJ5816 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Polystyrene |
3M Bumpon™ SJ5832 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to ABS |
3M Bumpon™ SJ5904 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Aluminum |
3M Bumpon™ SJ5908 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Stainless Steel |
3M Bumpon™ SJ6016 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Aluminum |
3M Bumpon™ SJ6016 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Stainless Steel |
3M Bumpon™ SJ6032 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 180°, Canvas to aluminum, pulled at 2"/min |
3M Scotch-Seal™ 2084 Metal Sealant Features: 3M™ Scotch-Seal™ Metal Sealant 2084 is a one-part aluminum colored sealant which air dries to a tough, flexible film that resists water, oils and fuel. Retains sealing properties after e.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | CRS, T-Peel, 17-20 mil bondline, MEK/abrade/MEK |
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Aluminum |
3M SJ5400 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Polypropylene |
3M SJ5500 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Polystyrene |
3M SJ5500 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Polystyrene |
3M SJ5700 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | Bond Strength; ASTM D624 |
Arlon 51576R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to ABS |
3M Bumpon™ SJ5916 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Stainless Steel |
3M Bumpon™ SJ5916 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Aluminum |
3M Bumpon™ SJ5916 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Polypropylene |
3M Bumpon™ SJ5808 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Polystyrene |
3M Bumpon™ SJ5808 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | T-Peel |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | CRS, T-Peel, 17-20 mil bondline, MEK/abrade/MEK |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | Al to Al |
Resinlab® EP1238 Acrylic / Epoxy Hybrid Adhesive Resinlab™ EP1238 is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wetting to.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | Al to Al |
Resinlab® EP1238 Black Acrylic / Epoxy Hybrid Adhesive Resinlab™ EP1238 Black is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wett.. |