Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.491 kN/m | 2.80 pli | Initial; ASTM D1000 |
Parker Chomerics CHO-FAB CRS Shielding Tape Conductive Adhesive Nickel-Plated FabricDescription: CHO-FAB® tape is a corrosion resistant nickel-plated cloth coated with Chomerics’ highly conductive pressure-sensitive adhesive. CHO-FAB® tape.. |
|||
Peel Strength | 0.491 kN/m | 2.80 pli | Initial; ASTM D1000 |
Parker Chomerics CHO-FOIL CCE Shielding Tape Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti.. |
|||
Peel Strength | 0.491 kN/m | 2.80 pli | Initial; ASTM D1000 |
Parker Chomerics CHO-FOIL CCH Shielding Tape Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti.. |
|||
Peel Strength | 0.491 kN/m | 2.80 pli | Initial; ASTM D1000 |
Parker Chomerics CHO-FAB CFT Shielding Tape Conductive Adhesive Nickel-Plated FabricDescription: CHO-FAB® tape is a corrosion resistant nickel-plated cloth coated with Chomerics’ highly conductive pressure-sensitive adhesive. CHO-FAB® tape.. |
|||
Peel Strength | 0.490 kN/m | 2.80 pli | to polyethylene, 180° peel test, rate of peel = 300mm/min at 25°C |
Kuraray SEPTON® A4 Hot Melt Adhesive Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. Using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo.. |
|||
Peel Strength | 0.491 kN/m | 2.80 pli | Bond Strength; MIL-I-46852C |
Arlon 915-10R##-P2 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular Certified to meet all requirements of US Military Specification A-A5.. |
|||
Peel Strength | 0.491 kN/m | 2.80 pli | Bond Strength; Arlon SQA-TMS-015 |
Arlon LW201R##-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: Level Wrap®: 1 inch wide, 20 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates.. |
|||
Peel Strength | 0.491 kN/m | 2.80 pli | Bond Strength; MIL-I-46852C |
Arlon LW201R##-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: Level Wrap®: 1 inch wide, 20 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates.. |
|||
Peel Strength | 0.491 kN/m | 2.80 pli | Bond Strength; MIL-I-46852C |
Arlon LW201R##-P2 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: Level Wrap®: 1 inch wide, 20 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates.. |
|||
Peel Strength | 0.491 kN/m | 2.80 pli | Bond Strength; Arlon SQA-TMS-015 |
Arlon LW401C##FR-P1 0.040" (1.02 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Brown, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Peel Strength | 0.491 kN/m | 2.80 pli | Glass, 180°, after 48 hrs at 23°C |
3M Fastbond™ 4224-NF Pressure Sensitive Adhesives 3M™ Fastbond™ Pressure Sensitive Adhesive 4224-NF is a water-based, permanently pressure sensitive adhesive with excellent initial tack and good bond strength.Information provided by 3M |
|||
Peel Strength | 0.491 kN/m | 2.80 pli | Clad Aluminum, 180°, after 48 hrs at 23°C |
3M Fastbond™ 49 Insulation Adhesive 3M™ Fastbond™ Insulation Adhesive 49 is a water-based, high solids, fast tacking, pressure sensitive adhesive for bonding lightweight materials like fiberglass insulation, felt, shoddy, paper and .. |
|||
Peel Strength | 0.491 kN/m | 2.80 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon R34570R005 0.005" (0.127 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 1080 Style FiberglassThis data represents typical values for the production material. The data should no.. |
|||
Peel Strength | 0.491 kN/m | 2.80 pli | Bond Strength; MIL-I-46852C |
Arlon 912-10X##-P0 0.012" (0.305 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 12 mil thick, Gray, Rectangular cross-section, Self-fus.. |
|||
Peel Strength | 0.491 kN/m | 2.80 pli | Bond Strength; MIL-I-46852C |
Arlon 915-10R##-P1 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular Arlon Rectangular Tape: Rectangular tape is of uniform thickness and.. |
|||
Peel Strength | 0.491 kN/m | 2.80 pli | Bond Strength; MIL-I-46852C |
Arlon 915-15X##-P0 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1.5” Wide Rectangular 1.5 inch wide, 15 mil thick, Gray, Rectangular cross-section, Self.. |
|||
Peel Strength | 0.491 kN/m | 2.80 pli | Bond Strength; Arlon SQA-TMS-015 |
Arlon T2040-B004 0.040" (1.02 mm) Cured Self-Fusing Silicone Rubber Description: 1 inch wide x 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone TapeDesign/Construction: Interleave: Polyester Product: Cured Self-Fusing Silicone RubberCross-Section:.. |
|||
Peel Strength | 0.491 kN/m | 2.80 pli | Bond Strength; MIL-I-46852C |
Arlon 915-10R##-P0 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular Arlon Rectangular Tape: Rectangular tape is of uniform thickness and.. |