Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchcal™ 5000 Reflective Graphic Film' 6-mil, enclosed lens, retroflective, flexible films; Pressure-sensitive adhesive; Permanent; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity w.. |
|||
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchcal™ IJ5000 Reflective Graphic Film' 6-mil, enclosed lens, retroflective, flexible films; Pressure-sensitive adhesive; Permanent; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity w.. |
|||
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 5100R Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Removable with heat; Available in 15 colors, including black (which ref.. |
|||
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 680CR-10 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 680CR-14 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 680CR-64 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 680CR-71 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 680CR-72 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 680CR-75 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 680CR-76 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 680CR-77 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 680CR-81 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 680CR-82 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ 680CR-85 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ IJ680CR-10 Removable Reflective Graphic Film with Comply™ Adhesive 6-mil flexible, enclosed lens, retoreflective films; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity when wet; Excellent angularity; Pressure-.. |
|||
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ RG5100R-10 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Removable with heat; Available in 15 colors, including black (which ref.. |
|||
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ RG680CR-10 Removable Reflective Graphic Film with Comply™ Adhesive 6-mil flexible, enclosed lens, retoreflective films; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity when wet; Excellent angularity; Pressure-.. |
|||
Peel Strength | 0.456 kN/m | 2.60 pli | Adhesion to Painted aluminum panels |
3M Scotchlite™ IJ5100R-10 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Removable with heat; Available in 15 colors, including black (which ref.. |