Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.438 kN/m | 2.50 pli | To Steel, Ambient Temperature; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4002 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Photopolymer, Adhesion; ASTM D3330 |
3M 414DL Flexomount™ Solid Printing Tapes 3M™ Flexomount™ Solid Printing Tapes are double coated tapes designed for mounting photopolymer and rubber printing plates to flexographic printing cylinders or sleeve systems. The adhesive system.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | HD Polypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330 |
3M 7014 Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7014FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | >= 0.438 kN/m | >= 2.50 pli | Bond Strength |
Arlon R35061R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Peel Strength | >= 0.438 kN/m | >= 2.50 pli | Bond Strength |
Arlon R35066R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 8654 Cold Temperature Reinforced Strapping Tape Scotch® Cold Temperature Reinforced Strapping Tape 8654 is a high performance, transparent packaging tape. This tape is reinforced along its length with continuous poly propylene monofilaments, whi.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7845TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7845TL is a matte clear polyester designed for sheet fed laser imprinting. This label material utilizes 3M™ Adhesive 310 which provides firmness .. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7880HL Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 78 lb clay-coated kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abras.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7880HL Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 78 lb clay-coated kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abras.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7881 Computer-Imprintable Polyester Label Material Features:Topcoated polyester is compatible with dot matrix printing and is hand writeable. The matte coating resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7883HL Computer-Imprintable Polyester Label Material Information provided by 3M |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7908FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7924 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7950 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | 90° Peel, PET/Stainless Steel, Initial (20 mins); ASTM D3330 |
3M 7993MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | 180° Peel 12"/min, 1" wide sample; TLMI Method |
3M P1510 Medical Permanent Acrylic Adhesives 3M™ Medical Permanent Acrylic Adhesives P1510 demonstrates excellent peel and tack performance and are designed for use in the medical attachment market.Information provided by 3M |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7730FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7742 Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Glass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7744 Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7840 Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Stainless Steel, 90° peel, 2 mil aluminum foil backing, 15 min at RT, 2.3 mil; ASTM D3330 |
3M 9555 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Adhesion to Steel; ASTM D3330 |
3M 97065 General Purpose Aluminum Foil Tape 60 lb. moisture stable liner. Good for die-cut applications.Information provided by 3M |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Stainless Steel, 90°, Silicone Adhesive, 15 min RT; ASTM D3330 |
3M 9731RW Double Coated Tape 3M™ Double Coated Tapes 9731 and 9731RW have a firm, silicone pressure sensitive adhesive coated on one side of a polyester film carrier and a high performance acrylic adhesive coated on the other .. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Adhesion to Steel; ASTM D3330 |
3M 33801 Premium Performance Aluminum Foil Tape High temperature acrylic adhesive of 425°F. UL 723 ClassifiedInformation provided by 3M |