Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.4163 kN/m | 2.375 pli | Stainless Steel, 180° Peel, Initial 10 min dwell at RT; ASTM D3330 |
3M 7737FL Velvet Textured Polycarbonate Overlaminating Film 3M™ Velvet Textured Polycarbonate Overlaminating Films 7737FL and 7738FL utilize velvet textured polycarbonate film to achieve a decorative velvet appearance. 3M™ Adhesive 400 offers excellent low.. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | Stainless Steel, 180° Peel, Initial 10 min dwell at RT; ASTM D3330 |
3M 7738FL Velvet Textured Polycarbonate Overlaminating Film 3M™ Velvet Textured Polycarbonate Overlaminating Films 7737FL and 7738FL utilize velvet textured polycarbonate film to achieve a decorative velvet appearance. 3M™ Adhesive 400 offers excellent low.. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7745FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Film 7745FL utilizes a matte clear polyester that is recommended for optimum durability and appearance in dot matrix and hand writable applications. The matte coating r.. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7745FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Film 7745FL utilizes a matte clear polyester that is recommended for optimum durability and appearance in dot matrix and hand writable applications. The matte coating r.. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | to Steel; ASTM D3330 |
3M Scotch® 231 Performance Masking Tape Scotch® Performance Masking Tape 231 is a premium high performance crepe paper masking tape designed to perform well in most industrial painting situations, including the use of bake cycles. This s.. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | Adhesion to Steel; ASTM D3330 |
3M 398FR Glass Cloth Tape 3M™ Glass Cloth Tape 398FR has an acrylic adhesive for many applications requiring high adhesion, an abrasion-resistant backing and flame retardant properties. This product is typically used for se.. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7880HL Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 78 lb clay-coated kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abras.. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7881 Computer-Imprintable Polyester Label Material Features:Topcoated polyester is compatible with dot matrix printing and is hand writeable. The matte coating resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations.. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7883 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Materials 7883 is a 3.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for tradition.. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7893 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7903FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7907 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat.. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7920 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7920 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. 3M™ Adhesive .. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7925 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7925 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7983 Sheet Polyester Label Material Features:Matte coating is compatible with screen printing and resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations. Variable information can be added by the end .. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7776 Polypropylene Label Material 3M™ Polypropylene Label Material 7776 is a durable polypropylene label stock that offers excellent performance in applications requiring surface conformability. This label product utilizes 3M™ Adh.. |
|||
Peel Strength | 0.4163 kN/m | 2.375 pli | Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7776 Polypropylene Label Material 3M™ Polypropylene Label Material 7776 is a durable polypropylene label stock that offers excellent performance in applications requiring surface conformability. This label product utilizes 3M™ Adh.. |