Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.40538 kN/m | 2.3125 pli | Polycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7745FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Film 7745FL utilizes a matte clear polyester that is recommended for optimum durability and appearance in dot matrix and hand writable applications. The matte coating r.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7840TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7850TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7200 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7200 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7845TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7845TL is a matte clear polyester designed for sheet fed laser imprinting. This label material utilizes 3M™ Adhesive 310 which provides firmness .. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7901 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Polycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7920 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7920 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. 3M™ Adhesive .. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | 90° Peel, PET/Stainless Steel, Initial (20 mins); ASTM D3330 |
3M 7951 Hi-Performance Acrylic 300MP This adhesive is designed for applications requiring greater initial adhesion especially to low surface energy (LSE) plastic substrates. Temperature performance is up to 300°F (149°C) for most app.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Adhesion to Steel; ASTM D3330 |
3M 1449 General Purpose Aluminum Foil Tape 1.4 mil backing; thin aluminum foil tape for conformability.Information provided by 3M |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Polycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7744 Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7884 White Vinyl Label Material Features:Conformable to contoured surfacesResists wrinkling and delaminationOne-piece removal up to one year after applicationTopcoated for impact printing, typewriters, ballpoint pens, pencils, and.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7902 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7902 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7906 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |