Polymer Property : Peel Strength = 16.9 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 2.96 kN/m
16.9 pli
Valley Adhesives EM-240 Low Temperature Application Glue Stick
Valley Adhesives EM-240 Low Temperature Application Glue StickBonds many woods and wood composites; Excellent for woodworking and cabinetry.