Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 2.52 kN/m | 14.4 pli | PP, 180° |
3M Scotch-Weld™ 6111HT Blue Bulk only Adhesive Same as 6111 but has higher heat resistance and blue in colorInformation provided by 3M |
|||
Peel Strength | 2.52 kN/m | 14.4 pli | PP, 180° |
3M Scotch-Weld™ 6111HT Tan Bulk only Adhesive Same as 6111 but has higher heat resistanceInformation provided by 3M |