Polymer Property : Peel Strength = 13.7 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 2.40 - 3.20 kN/m
13.7 - 18.3 pli
ISO 4578
Permabond ET505 Epoxy Resin
PERMABOND ET505 is a two-part, 1:1 mixable epoxy adhesive. ET505 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas..
Peel Strength 2.40 - 3.20 kN/m
13.7 - 18.3 pli
ISO 4578
Permabond ET515 Epoxy Resin
PERMABOND® ET515 is a 1:1 mixable epoxy adhesive. ET515 is a semi-flexible toughened adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo..
Peel Strength 2.40 - 3.20 kN/m
13.7 - 18.3 pli
ISO 4578
Permabond ET536 Epoxy Resin
PERMABOND ET536 is a two-part, 1:1 mixable epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and composites. Permabond ET536 forms tough bo..