Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NH9294 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NH9300 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NH9320 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NH9338 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NH9348 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NH9350 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NH9410 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NH9450 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9240 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9245 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9250 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9255 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9260 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9270 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9294 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9300 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9320 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NY9208 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NY9217 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NY9220 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | 18, 35, and 70µm copper; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NY9233 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | After 2 week exposure to 71°C, Vinyl-Altro to Composite, 2 surface Bond |
3M Scotch-Weld™ 4491 Vinyl Bonding Cylinder Spray Adhesive Industrial grade, high performance, plasticizer resistant bulk spray adhesive formulated for bonding vinyl. The adhesive is available in a convenient, portable, no maintenance aerosol cylinder.Infor.. |
|||
Peel Strength | 2.33 kN/m | 13.3 pli | (S1 to S1), Bond Strength; Arlon SQA-TMS-011 |
Arlon 55279R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |
|||
Peel Strength | 2.33 kN/m @Temperature 23.0 °C |
13.3 pli @Temperature 73.4 °F |
Aluminum, etched, Bell Peel, Adhesive Failure; ASTM D3167 |
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives 3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f.. |