Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 8.77 kN/m | 50.0 pli | Tensile |
Dielectric Polymers NT-4512 High Temperature Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film. For applicati.. |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | Tensile |
Dielectric Polymers NT-2821 Ultra Tack Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film at zero wet out.. |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | Tensile |
Dielectric Polymers NT-2821-2 Ultra Tack Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film at zero wet out.. |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | Tensile |
Dielectric Polymers NT-2822 Ultra Tack Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film at zero wet out.. |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | Tensile |
Dielectric Polymers NT-2012-2 Photo Processing Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing photographic film to leader card during film proc.. |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | Tensile |
Dielectric Polymers NT-5521-2 Photo Processing Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing photographic film to leader card during film proc.. |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | Tensile |
Dielectric Polymers NT-8512-2 Photo Processing Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing photographic film to leader card during film proc.. |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | Tensile |
Dielectric Polymers NT-702 Acrylic Tape
(discontinued **) Acrylic adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of non-silicone coated substrates. Provides high temperature s.. |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | Tensile |
Dielectric Polymers NT-5000 Protective Film
(discontinued **) Acrylic adhesive with polyester film backing.Features: Clean removal even after exposure to high and low temperaturesSolvent resistantMoisture resistantFor use on matte metals and textured plasticsA.. |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | Tensile |
Dielectric Polymers NT-8512-2 Powder Coating Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityNo film shrinkage after exposure to elevated temperaturesAbrasion resista.. |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | Tensile |
Dielectric Polymers NT-9512 Powder Coating Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityNo film shrinkage after exposure to elevated temperaturesAbrasion resista.. |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | Tensile |
Dielectric Polymers NT-9512-2DL Selective Masking Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: High temperature resistantDie cut disks/shapes remove easily from linerClean tape removalApplications: For selective masking appli.. |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | |
ITW Devcon Flex Bondâ„¢ Methacrylate Adhesive Pipe Sealant, Purple Information provided by ITW Devcon |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | |
ITW Devcon Safety Clear Coatâ„¢ Epoxy, Water Clear Information provided by ITW Devcon |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | At 100% cohesive failure using 1 in. x 8 in. stainless steel screen at 180° pull angle |
Momentive Performance Materials RTV1673LV One Component, Low Volatile Silicone Adhesive Sealant, Black RTV1673LV one-component, ready-to-use adhesive sealants cures to a tough durable, resilient silicone rubber when exposed to atmospheric moisture at room temperature. Methyl alcohol and a small amoun.. |
|||
Peel Strength | 8.77 kN/m @Temperature 21.1 °C |
50.0 pli @Temperature 70.0 °F |
|
Hexcel® Redux® 335U Adhesive film for bonding metallic and composite components (0.06 psf) Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a.. |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | Aluminum Etched, T-Peel, 17-20 mil bondline |
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Peel Strength | 8.77 kN/m @Temperature 23.0 °C |
50.0 pli @Temperature 73.4 °F |
Aluminum, T-Peel |
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | T-Peel, CRS Oakite degreased, 5-8 mil bondline |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | Solvent Wiped T-Peel |
3M Scotch-Weld™ EC-2086 Structural Adhesive 3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | 180°, Polystyrene |
3M Scotch-Weld™ TS230 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | 180°, Polyacrylic |
3M Scotch-Weld™ EZ250150 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th.. |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | 180°, Aluminum |
3M Scotch-Weld™ EZ250150 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th.. |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | Aluminum Etched, T-Peel, 5-8 mil bondline |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Peel Strength | 8.77 kN/m @Temperature 23.0 °C |
50.0 pli @Temperature 73.4 °F |
Aluminum, T-Peel |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Peel Strength | 8.77 kN/m | 50.0 pli | Tensile |
Dielectric Polymers NT-5002 Protective Film
(discontinued **) Acrylic adhesive with polyester film backing.Features: Clean removal even after exposure to high and low temperaturesSolvent resistantMoisture resistantFor use on matte metals and textured plasticsA.. |