Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 7.36 kN/m | 42.0 pli | Tensile |
Dielectric Polymers NT4500 Protective Film
(discontinued **) Acrylic adhesive with polyester film backing.Features: Clean removal even after exposure to high and low temperaturesSolvent resistantMoisture resistantFor use on matte metals and textured plasticsA.. |
|||
Peel Strength | 7.36 kN/m | 42.0 pli | Tensile |
Dielectric Polymers NT-4502 Protective Film
(discontinued **) Acrylic adhesive with polyester film backing.Features: Clean removal even after exposure to high and low temperaturesSolvent resistantMoisture resistantFor use on matte metals and textured plasticsA.. |
|||
Peel Strength | 7.36 kN/m | 42.0 pli | Glass |
Momentive Performance Materials RTV5812 One-Component, Modified Alkoxy Adhesive Sealant, White RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Peel Strength | 7.36 kN/m | 42.0 pli | Glass |
Momentive Performance Materials RTV5813 One-Component, Modified Alkoxy Adhesive Sealant, Black RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Peel Strength | 7.36 kN/m | 42.0 pli | Glass |
Momentive Performance Materials RTV5818 One-Component, Modified Alkoxy Adhesive Sealant, Translucent RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |