Polymer Property : Peel Strength = 7.01 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 7.01 kN/m
40.0 pli
Aluminum, Cold Rolled Steel, Epoxy, Rigid PVC
Momentive Performance Materials N-Sil® RTV122 Silicone Modified Alkoxy Adhesive Sealants, White
N-Sil® adhesive sealants are one-component, ready-to-use, and cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature.Key Performance Properties: Primer..
Peel Strength 7.01 kN/m
40.0 pli
Aluminum, Cold Rolled Steel, Epoxy, Rigid PVC
Momentive Performance Materials N-Sil® RTV123 Silicone Modified Alkoxy Adhesive Sealants, Black
N-Sil® adhesive sealants are one-component, ready-to-use, and cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature.Key Performance Properties: Primer..
Peel Strength 7.01 kN/m
40.0 pli
Aluminum, Cold Rolled Steel, Epoxy, Rigid PVC
Momentive Performance Materials N-Sil® RTV128 Silicone Modified Alkoxy Adhesive Sealants, Translucent
N-Sil® adhesive sealants are one-component, ready-to-use, and cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature.Key Performance Properties: Primer..
Peel Strength 7.01 kN/m
40.0 pli
At 100% cohesive failure using 1 in. x 8 in. stainless steel screen at 180° pull angle
Momentive Performance Materials RTV102 One Component Acetoxy Adhesive Sealant, White
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Peel Strength 7.01 kN/m
40.0 pli
At 100% cohesive failure using 1 in. x 8 in. stainless steel screen at 180° pull angle
Momentive Performance Materials RTV103 One Component Acetoxy Adhesive Sealant, Black
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Peel Strength 7.01 kN/m
40.0 pli
At 100% cohesive failure using 1 in. x 8 in. stainless steel screen at 180° pull angle
Momentive Performance Materials RTV106 One Component Acetoxy Adhesive Sealant, Red
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Peel Strength 7.01 kN/m
40.0 pli
At 100% cohesive failure using 1 in. x 8 in. stainless steel screen at 180° pull angle
Momentive Performance Materials RTV108 One Component Acetoxy Adhesive Sealant, Translucent
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Peel Strength 7.01 kN/m
40.0 pli
At 100% cohesive failure using 1 in. x 8 in. stainless steel screen at 180° pull angle
Momentive Performance Materials RTV109 One Component Acetoxy Adhesive Sealant, Aluminum
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Peel Strength 7.01 kN/m
40.0 pli
1 in. x 8in. Stainless steel screen at 180° pull angle
Momentive Performance Materials RTV162 Electronic Grade Silicone Adhesive Sealant, White
RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm..
Peel Strength 7.01 kN/m
40.0 pli
Lexan Polycarbonate®
Momentive Performance Materials RTV5812 One-Component, Modified Alkoxy Adhesive Sealant, White
RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature...
Peel Strength 7.01 kN/m
40.0 pli
Lexan Polycarbonate®
Momentive Performance Materials RTV5813 One-Component, Modified Alkoxy Adhesive Sealant, Black
RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature...
Peel Strength 7.01 kN/m
40.0 pli
Lexan Polycarbonate®
Momentive Performance Materials RTV5818 One-Component, Modified Alkoxy Adhesive Sealant, Translucent
RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature...
Peel Strength 7.01 kN/m
40.0 pli
Cure cycle: 1 day @ RT, with Acid Etched 6061-T6 Aluminum
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Liquid
Epovex® Adhesive is a carbon nanotube enhanced ambient or elevated temperature cure two-part epoxy adhesive. Used for bonding, laminating, filling or potting, Epovex is ideal for many metals, woods..
Peel Strength 7.01 kN/m
40.0 pli
Cure cycle: 12 hrs @ RT + 1 hr @ 176°F, with Acid Etched 6061-T6 Aluminum
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Liquid
Epovex® Adhesive is a carbon nanotube enhanced ambient or elevated temperature cure two-part epoxy adhesive. Used for bonding, laminating, filling or potting, Epovex is ideal for many metals, woods..
Peel Strength 7.01 kN/m
40.0 pli
Cure cycle: 3 days @ RT, with Acid Etched 6061-T6 Aluminum
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Liquid
Epovex® Adhesive is a carbon nanotube enhanced ambient or elevated temperature cure two-part epoxy adhesive. Used for bonding, laminating, filling or potting, Epovex is ideal for many metals, woods..
Peel Strength 7.01 kN/m
40.0 pli
Cure cycle: 12 hrs @ RT + 1 hr @ 176°F, with Acid Etched 6061-T6 Aluminum
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Paste
Epovex® Adhesive Paste is a carbon nanotube enhanced two part epoxy adhesive thixotropic paste. Used for bonding or filling, Epovex Paste is ideal for many metals, woods, masonry products, and some..
Peel Strength 7.01 kN/m
40.0 pli
Aluminum Etched, T-Peel, 5-8 mil bondline
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Peel Strength 7.01 kN/m
40.0 pli
CRS, T-Peel, 17-20 mil bondline, Oakite degreased
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Peel Strength 7.01 kN/m
40.0 pli
T-Peel, CRS MEK/abrade/MEK, 5-8 mil bondline
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Peel Strength 7.01 kN/m
40.0 pli
Adhesion to Aluminum
3M EPS-200 Tubing
3M EPS-200 is a 2:1 thin-wall tubing offering the advantages of integral adhesive-lined construction. The tubing is made from a flame-retardant, flexible polyolefin with a thing layer of special the..
Peel Strength 7.01 kN/m
40.0 pli
Adhesion to Aluminum
3M EPS-300 Heat Shrink Tubing
3M Heat Shrink tubing EPS-300 is a 3:1 thin-wall, flexible tubing offering the advantages of integral, adhesive-lined construction. The tubing is made from flame-retardant, flexible polyolefin with ..
Peel Strength 7.01 kN/m
40.0 pli
Adhesion to Aluminum
3M EPS-400 Heat Shrink Tubing
3M Heat Shrink tubing EPS-400 is a medium-wall, semi-rigid tubing offering the advantages of integral, adhesive-lined construction. The tubing is made from flame-retardant, flexible polyolefin with ..
Peel Strength 7.01 kN/m
40.0 pli
CRS, T-Peel, 17-20 mil bondline, Oakite degreased
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Peel Strength >= 7.01 kN/m
>= 40.0 pli
Tensile, Al to Al
Master Bond Supreme 10HTFL One Part Epoxy Cures at 250°F
Description: Master Bond Polymer System Supreme 10HTFL features a blend of physical properties including outstanding peel strength, very high shear strength and a wide service temperature range of 4..
Copyright © lookpolymers.com All Rights Reserved