Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 4.21 kN/m | 24.0 pli | Bond Strength; ASTM D624 |
Arlon 55578XA030 0.032" (0.813 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: 162 Style Fiberglass Side 1: Cured Silicone Rubber (Skim Coat).. |