Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 3.40 - 4.00 kN/m | 19.4 - 22.8 pli | ISO 4578 |
Permabond TA435 Toughened Acrylic Adhesive & Initiator PERMABOND TA435 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This adhesive may be used in a variety of structural bonding appli.. |
|||
Peel Strength | 3.40 - 4.00 kN/m | 19.4 - 22.8 pli | ISO 4578 |
Permabond TA437 Toughened Acrylic Adhesive PERMABOND TA437 is a single component structural acrylic adhesive designed primarily for bonding metals, ferrites and ceramics. The typical fixture time of TA437 when used with Initiator 41 is 30 –.. |
|||
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-120H TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Max. toluene solubility, MC solubleExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Use.. |
|||
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-620 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-626 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-626H TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-626L TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-626SH TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-626SL TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-690 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Peel Strength | 3.40 - 5.44 kN/m | 19.4 - 31.0 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-690H TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Peel Strength | 3.40 kN/m | 19.4 pli | Mylar Film; ASTM D-1876-72 |
Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane Features: Soft compound with high elongation, displays low temperature flexibility and abrasion resistance. It can be processed by means of solution coating, extrusion and melt coating.Uses: Adhesiv.. |
|||
Peel Strength | 3.40 kN/m | 19.4 pli | T-Peel (CRS St 1203, 0.5mm) |
Dow BETAMATE™ 1045 Epoxy BETAMATE™ 1045 is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excellent.. |
|||
Peel Strength | 3.40 kN/m | 19.4 pli | Impact Peel |
Dow BETAMATE™ 5103-2 Epoxy BETAMATE™ 5103-2 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel, including coated ste.. |