Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 2.07 kN/m
11.8 pli
Silicone to FEP Bond Strength
Arlon 22122R079 0.079" Cured Silicone Rubber and FEP Film Laminate
Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: 0.005" FEP FilmThis data represents typical values for the production material and should not be used as ..
Peel Strength 2.07 kN/m
11.8 pli
Silicone to FEP Bond Strength; Arlon SQA-TMS-011
Arlon R37732R079 0.079" (2.01 mm) Cured Silicone Rubber with FEP Film Substrate
Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: FEP FilmAppearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical value..
Peel Strength 2.07 kN/m
11.8 pli
Silicone to FEP Bond Strength; Arlon SQA-TMS-011
Arlon R37732W079 0.079" (2.01 mm) Cured Silicone Rubber with Treated FEP Film Substrate
Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: Treated FEP FilmThis data represents typical values for the production material. The data should not be used to w..