Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Peel Strength = 101 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 101 kN/m
576 pli
Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
3M 7603 Clear Vinyl Label Material
3M™ Clear Vinyl Label Material 7603 is a soft, flexible vinyl film with excellent durability. This label material utilizes 3M™ High Strength Acrylic Adhesive 300, which has excellent quick tack an..